Add to Cart
![]() | ![]() |
Hot Forging SS316 Rigid Axle Stainless Steel Shaft Forging
1. Name: Stainless steel forging shaft
2. Material: Carbon steel alloy steel or stainless steel
3. Certificates: ISO9001-2008, PED
4. Min order: 1 PCS
5. Payment times: T/T OR L/C
6. Delivery time: 1piece needs 30days(normal size)
7. Forged process: Hot forged N or Q+T
8. Size: Big size or customers requipment
9. Packing: In wooden cases, wooden pallets or as per customers' special requirement;
10. Price: FOB10-100USD/PC
11. OD3000MM, LENGTH 10000MM;
12. Weight from 100 kg to 50000kg;
Packaging & Delivery
Packaging Details:Delivery Detail:
wooden or steel package seaworthy packing |
about 35 days from order or as per customer requirement |
FAQ
1.Trade term:FOB/CIF/CFR.
2.Payment term:T/T or L/C.
3.Inquiry: Please show me drawings and detail technical specifications
4.Delivery Detail:about 35 days from order.
Item | Process | Facility | Inspection items | Standard |
01 | Steel material inspection | Chemical composition (EF+LF+VD) | Material standard | |
surface | Ingot inspection specification | |||
Ingot type and weight | Material standard | |||
02 | Material store | Division put | warehouse management | |
1 | Heat | Heat furnace | Temperature/Time | Heating process specification Forging production procedure |
2 ↓ | Forging | Press | Reduction ratio,forging temperature,deformation, Surface and dimensions | Forging process card Forging procedure |
3 ↓ | Heat treatment | heat treatment furnace | heat treatment charts | 1st heat-treatment card Forging procedure |
4 ↓ | Rough inspection | Dimensions, apperance, Mark | Inspection specification Forging procedure | |
5 ↓ | Rough UT | UT equipment | Single defect, concentrated Defects bottom wave attenuation | UT standard or customer's technical requirements |
6 ↓ | Saw cutting | Saw machine | Dimension | IQC and forging |
7 ↓ | rough turning | turning-lathe | Dimension,appearance | Rough machining drawing |
8 ↓ | UT | UT equipment | Single defect, concentrated defects bottom wave attenuation | UT standard or customer's technical requirements |
9 ↓ | Q+T heat treatment | heat treatment furnace | heat treatment charts | Heating process specification |
10 ↓ | Sampling or machining | machining tool | rough machining drawing sampling drawing | sample machining drawing |
11 ↓ | mechanical property test | tensile testing machine/ impact testing machine | ambient temperature,humidity, Test temp.Sample dimension, test method | Standard technical specification |
12 ↓ | finish machining | machining tool | Dimension,appearance | finish machining drawing |
13 ↓ | UT | UT equipment | Single defect, concentrated Defects bottom wave attenuation | UT standard or customer's technical requirements |
14 ↓ | MT | MT equipment | Magnetic particle indication | Test standard or Technical requirements |
15 ↓ | Mark | Steel seal | marking content | Product standard Technical requirements Forging process |
16 ↓ | Final inspection | Appearance, dimension, mark acceptance inspection | Product inspection specification Product standard P.O. | |
17 | Protection/ package | Blasting Blasting equipment | appearance coating thickness | Product standard Technical requirements |